# Body Armour

> Scales, mail, plate and fibre to stop a blow

- Date: c. 2,100 BCE
- Era: Antiquity
- Domain: [Defence & Fortification](https://lastcodex.org/en/domains/defense/)
- Rebuild stage: III (Crafts & cities)
- Difficulty: 3/5
- URL: https://lastcodex.org/en/inventions/body-armor/

Body armour is clothing that takes a blow in place of the body. The oldest known pieces are armour plates of bone and horn from graves at Rostovka, in western Siberia, dated to about 2100 BC. Coats of bronze scales laced onto linen or leather were worn by chariot warriors in the Near East in the 15th century BC. Mail of interlinked iron rings followed around 300 BC, then suits of steel plate in late medieval Europe, and in the 1970s vests of synthetic fibre tested against firearms to official standards.

![Body Armour · Scales, mail, plate and fibre to stop a blow](https://lastcodex.org/_astro/plate.44h8UKPD_Z15pRCe.webp)

## Legend

1. Short sleeve
2. Bronze scale
3. Strengthening ridge
4. Lacing
5. Linen or leather backing

## What it is

Body armour is a garment that takes the force of a weapon so that the body behind it does not. It has been made of many materials: small plates of bone, [bronze](/en/inventions/bronze/) or iron sewn onto cloth, rings of iron wire linked into a flexible mesh, shaped plates of [steel](/en/inventions/steel/), quilted cloth, and in recent decades woven synthetic fibres. Soldiers have usually combined several of these, with a soft padded layer under a hard one.

A coat of bronze scales of the type worn in the Near East in the 15th century BC, known from scales found at Nuzi in Iraq and coats painted in Egyptian tombs, reaches the knees and has short sleeves. Each scale is a small bronze plate, square at the top and rounded at the bottom, with a ridge pressed along its middle to stiffen it and small holes for the laces. The scales are laced side by side into rows, and the rows are sewn onto a garment of linen or leather so that each row hangs over the top of the row below.

## How it works

A hard surface turns or spreads the point of a weapon: an arrow or a blade that strikes a bronze scale or a steel plate either glances off or has its force spread over a larger area. In a scale coat the scales overlap, so a weapon meets several thicknesses of metal, and the laces lie hidden under the scales and under the row above, where they are hard to cut. A coat took a great many scales: Thomas David Hulit cites Walter Ventzke's estimate of about 1,300 for a short sleeveless corslet and more than 3,300 for a long coat.

![A square of riveted iron mail lying on a wooden block: rows of flat solid rings alternate with rows of rings closed by a small rivet, each ring passing through its neighbours](https://lastcodex.org/_astro/v1.DDls_ECU_ZwFIQe.webp)
_In this riveted mail, rows of solid rings alternate with rows of rings closed by a rivet._

Mail is a mesh of small iron rings, each passing through its neighbours. Some rings were closed with a rivet, others were forge-welded or punched whole from sheet metal. Mail bends with the body and resists cuts. It was worn over a padded tunic of cloth stuffed with wool or cotton, which softened the blows. Egyptian soldiers of the New Kingdom also wore armour of padded linen on its own.

Plate armour shapes steel to the body. Where the body bends, at the elbows, knees and waist, narrow overlapping strips of steel called lames are joined by rivets and leather straps so that they can slide over one another. The Metropolitan Museum of Art gives 20 to 25 kg for a complete field armour, spread over the whole body instead of hanging from the shoulders. In 2024 a team led by Andreas Flouris had Greek marines wear a replica of the Bronze Age Dendra armour through an 11-hour simulated battle and found it allowed full movement without excessive physical strain.

Modern vests use many layers of very strong synthetic fibre. In the United States they are tested in independent laboratories against the standard of the National Institute of Justice, and each model is certified for stated threats. The institute warns that no armour is bulletproof: a vest protects only against the threats it was chosen and tested for.

## How to do it

A small sample of scale armour made of card shows how the scales overlap and hide their laces. It protects against nothing. You need thin card such as a cereal box, a ruler and pencil, scissors, a hole punch, thin string or embroidery thread, a darning needle and a piece of felt about 15 cm square.

![A small sample: rows of card scales with rounded ends, punched with holes, laced together with string and sewn onto a square of grey felt, with scissors, a hole punch and a few punched-out discs beside it](https://lastcodex.org/_astro/v2.RJw2wk5V_Ztj0id.webp)
_On the card sample each row of scales is laced through its holes and overlaps the row below._

Cut about thirty card scales, each 2 cm wide and 4 cm long, square at the top and rounded at the bottom. Punch two holes side by side near the top of each scale. Lay ten scales in a row, edges slightly overlapping, and thread the string through the holes to lace them together. Make three rows this way. Sew the lowest row to the bottom of the felt through its lacing, then sew the next row about 2 cm higher so that its scales cover the top of the first row and its laces, and do the same with the third row. Bend the felt and see how the scales slide over one another.

> **Safety.** A card or metal sample of this kind gives no protection at all; only equipment certified to a recognised standard, worn as its maker instructs, protects against weapons.

## History and evolution

The oldest known body armour comes from western Siberia. At Rostovka, near Omsk, graves furnished with bronze weapons of the Seima-Turbino type also held stone casting moulds and armour plates of horn, and grave 34 contained body armour of bone. Radiocarbon dates published in 2017 by Zinaida Marchenko and colleagues place these graves between the 22nd and the 20th centuries BC. The authors warn that human bone from the region can give dates that are too old, and earlier studies based on the style of the bronzes had put them in the 16th and 15th centuries BC.

The oldest armour scales found with written records come from Nuzi, near Kirkuk in northern Iraq. Excavators found bronze scales in houses of the town, dated to about 1475 to 1450 BC, together with clay tablets listing the armour issued to the soldiers of the palace: coats of large and small copper scales, sleeves, skirts, helmets and also corslets of leather. Scale armour was costly, and Timothy Kendall, who studied the tablets, thought that only elite units, officers and the wealthy owned coats with metal scales. When Thutmose III of Egypt defeated a coalition of Syrian and Canaanite princes at Megiddo in the 15th century BC, his annals list among the booty one fine bronze coat of armour belonging to the enemy leader, one belonging to the prince of Megiddo, and 200 coats of the defeated army. The Metropolitan Museum of Art holds bronze armour scales excavated at Malqata, the palace of Amenhotep III, from about 1386 to 1347 BC.

In Greece a different kind of armour has survived. The Dendra panoply, found in 1960 in a chamber tomb near Mycenae and about 3,500 years old, is a full suit of large shaped bronze plates. Its original weight is estimated at about 18 kg.

Mail appeared much later, among the Celts of central Europe. A chieftain's grave found by chance in 1961 at Ciumeşti in Romania held an iron helmet crowned with a bird of prey, a coat of iron mail and bronze greaves, from the 3rd century BC. Czech researchers now place the invention of mail at the turn of the 4th and 3rd centuries BC and treat the Ciumeşti coat, whose rings are simply butted together, as an early example but not the earliest.

![A complete suit of 15th-century steel plate armour on a wooden stand: visored helmet, breastplate, shoulder defences, jointed elbows and knees, gauntlets and pointed steel shoes](https://lastcodex.org/_astro/v3.BhL2-3GB_6Wf1R.webp)
_By the second quarter of the 15th century a knight could be covered in steel from head to foot._

In medieval Europe riveted mail over a padded tunic was the main armour for centuries. Steel plates were added over the mail during the 14th century, and from the second quarter of the 15th century a fully armed knight was covered in plate from head to foot, with a padded arming doublet underneath.

In 1965 the chemist Stephanie Kwolek at DuPont discovered the fibre later sold as Kevlar. In 1972 the predecessor of the US National Institute of Justice published the first performance standard for police body armour. In 1975 and 1976 about 5,000 Kevlar vests were tried in the field by 15 police agencies in cities across the country, and in 1978 the institute set up compliance testing: a maker may not label a model as meeting the standard until it has passed the tests. The standard has been revised several times since, most recently as NIJ Standard 0101.07, published in 2023.

## Key facts

- Oldest known armour plates: Bone and horn, graves at Rostovka near Omsk, Siberia, 22nd to 20th century BC
- Booty taken at Megiddo by Thutmose III, 15th century BC: Two fine bronze coats of armour and 200 coats from the defeated army
- Dendra panoply, found near Mycenae in 1960: Bronze plates, the original estimated at about 18 kg
- Complete steel plate armour, 15th century AD: About 20 to 25 kg, spread over the whole body
- First US standard for police body armour: 1972; the current version, 0101.07, was published in 2023

## Requires

- [Bronze](https://lastcodex.org/en/inventions/bronze/): Copper and tin, harder together (c. 3,300 BCE)
- [Weaving](https://lastcodex.org/en/inventions/weaving/): Threads crossed into cloth (c. 6,700 BCE)
- [Needle and hand sewing](https://lastcodex.org/en/inventions/needle-and-hand-sewing/): A polished eye carries the thread (40,000 years ago)

## Sources

- [Radiocarbon Chronology of Complexes With Seima-Turbino Type Objects (Bronze Age) in Southwestern Siberia](https://doi.org/10.1017/RDC.2017.24), Radiocarbon 59 (Marchenko, Svyatko, Molodin, Grishin and Rykun, 2017)
- [Bronze age Northern Eurasian genetics in the context of development of metallurgy and Siberian ancestry](https://doi.org/10.1038/s42003-024-06343-x), Communications Biology 7 (Childebayeva et al., 2024)
- [Late Bronze Age Scale Armour in the Near East (PhD thesis)](https://etheses.durham.ac.uk/id/eprint/1006/), Durham University (Thomas David Hulit, 2002)
- [The Annals of Thutmose III: the Battle of Megiddo](https://sourcebooks.web.fordham.edu/ancient/1469BC-egypt-megiddo.asp), Internet Ancient History Sourcebook, Fordham University (J. H. Breasted translation)
- [How a single battle, and one young pharaoh, turned Egypt into a superpower](https://www.nationalgeographic.com/history/article/thutmose-ancient-egypt-pharaoh-military-leader), National Geographic (Javier Martínez Babón, 2025)
- [Scale from Armor, Malqata, reign of Amenhotep III](https://www.metmuseum.org/art/collection/search/577194), The Metropolitan Museum of Art
- [Analysis of Greek prehistoric combat in full body armour based on physiological principles](https://journals.plos.org/plosone/article?id=10.1371/journal.pone.0301494), PLOS ONE 19 (Flouris et al., 2024)
- [These modern soldiers put Bronze Age armor to the test](https://www.nationalgeographic.com/premium/article/greece-armor-mycenaean-dendra-illiad-bronze-age), National Geographic, 2024
- [Ciumeşti. Ghid cultural şi istoric](https://library.hungaricana.hu/en/view/SzatmariMuzeumKiadvanyai_Ghiduri_Ghid_cultural_Giumesti-Csomakoz/?pg=14), Satu Mare County Museum, 2010 (Hungaricana)
- [Research result on the Ciumeşti mail coat and the invention of mail](https://starfos.tacr.cz/vysledky-vyzkumu/RIV%2F68081758%3A_____%2F25%3A00639040), Institute of Archaeology of the Czech Academy of Sciences (Starfos, 2025)
- [Ciumeşti helmet may be exhibited at the National Museum of Romanian History](https://agerpres.ro/english/2026/05/06/ciumesti-helmet---may-exhibit-at-the-national-museum-of-romanian-history--1553527), Agerpres, 2026
- [The Armour of an English Medieval Knight](https://www.worldhistory.org/article/1244/the-armour-of-an-english-medieval-knight/), World History Encyclopedia (Mark Cartwright, 2018)
- [Arms and Armor: Common Misconceptions and Frequently Asked Questions](https://www.metmuseum.org/essays/arms-and-armor-common-misconceptions-and-frequently-asked-questions), The Metropolitan Museum of Art, Heilbrunn Timeline of Art History
- [Mail shirt](https://worcester.emuseum.com/objects/49673/mail-shirt), Worcester Art Museum
- [Mail armour from the collection of the National Museum of Slovenia](https://www.nms.si/en/exhibitions/12127-Mail-armour-from-the-collection-of-the-National-Museum-of-Slovenia), National Museum of Slovenia
- [Stephanie L. Kwolek](https://www.sciencehistory.org/education/scientific-biographies/stephanie-l-kwolek/), Science History Institute
- [NIJ's Bullet-Resistant Vest Standard Reaches Milestone](https://www.ojp.gov/pdffiles1/jr000249e.pdf), NIJ Journal 249, National Institute of Justice, 2003
- [Body Armor: Protecting Our Nation's Officers From Ballistic Threats](https://nij.ojp.gov/topics/articles/body-armor-protecting-our-nations-officers-ballistic-threats), National Institute of Justice, 2018
- [Technology 70s Style: NIJ at the Forefront of Body Armor Research and Development](https://nij.ojp.gov/library/publications/technology-70s-style-nij-forefront-body-armor-research-and-development), National Institute of Justice
- [Ballistic Resistance of Body Armor, NIJ Standard 0101.07](https://nij.ojp.gov/topics/equipment-and-technology/ballistic-resistance-body-armor-nij-standard-010107), National Institute of Justice

Fact-checked on 2026-10-19.

---

The Last Codex · https://lastcodex.org/en/inventions/body-armor/ · © The Last Codex. Texts, plates and figures: CC BY-NC-ND 4.0.