# Gelatin production

> Dissolving the collagen of skin and bone in hot water, then setting and drying it

- Date: c. 8,430 BCE
- Era: Prehistory
- Domain: [Materials & Chemistry](https://lastcodex.org/en/domains/materials/)
- Rebuild stage: II (Settlement)
- Difficulty: 2/5
- URL: https://lastcodex.org/en/inventions/gelatin-production/

Gelatin is the collagen of skin, bone and fish skin taken apart by heat and dissolved in hot water. The raw material is first steeped to loosen it, the warm extract is cleared and thickened, and on cooling it sets into a jelly that is then dried. Crude gelatin is hide glue. In the cave of Nahal Hemar, in Israel, a coating of collagen and plant resin on a human skull has been dated directly to 8920 to 8430 BCE, and baskets from the same layer are lined with cattle collagen.

![Gelatin production · Dissolving the collagen of skin and bone in hot water, then setting and drying it](https://lastcodex.org/_astro/plate.D-t-q0yv_Z3SWqT.webp)

## Legend

1. Vat where skin parings soak in lime water
2. Copper cauldron over the fire, where the collagen dissolves
3. Cloth-lined basket that strains the liquor
4. Box where the cooled liquor sets into jelly
5. Slices of jelly drying on nets

## What it is

Gelatin is a protein obtained from collagen, the fibrous protein that makes skin tough and gives bone its spring. Collagen does not dissolve in water, but long heating in water takes it apart into shorter, looser chains that do. That solution, cleared and thickened, sets into a jelly when it cools and dries into hard, clear sheets or grains. Those dried pieces are gelatin.

The same substance, less purified, is the oldest glue made from animals. Glue makers boiled parings of hide and sinews, and their brown cakes of hide glue are a crude gelatin. Refined gelatin goes into jellies and sweets, into capsules for medicines and, from the 1870s, into photographic film and paper.

The raw materials are by-products of meat and leather. In Europe most gelatin now comes from pig skin, and most of the rest from the split inner layer of cattle hide, with a little from bones and fish.

## How it works

![Model of a three-strand cord in three colours on a wooden table: on the left the three strands are twisted tightly into a helix, towards the right they come apart into three loose, wavy strands](https://lastcodex.org/_astro/v1.HOgPThra_Z1lHmQA.webp)
_Collagen is a tight triple helix; heat in water unwinds it into loose chains of gelatin._

Collagen is built from three protein chains wound round one another in a stiff helix. In skin and bone, these helices are packed into fibres and tied to their neighbours by many chemical links, which is why a hide can be soaked for days without dissolving. To make gelatin, those links must first be loosened.

That is the purpose of the steeping. Cattle hides and bones are usually soaked for several weeks in an alkaline bath of lime, pig skins for about a day in a dilute acid. The collagen swells, some links break, and fat, hair and other proteins are washed away. Bones are also stripped of their minerals first, which leaves the soft collagen of the bone.

Hot water does the rest. The steeped material is heated in water in several stages, each hotter than the last, and the helices unwind and the freed chains go into solution. The first, gentlest extractions give the firmest jelly; the later, hotter ones give weaker grades. Glue makers did the same in one cauldron, drawing off the liquor in batches.

The warm liquor is then filtered, cleared of fat and salts, and thickened by evaporating water, in modern plants under vacuum, until it is as thick as honey. It is sterilised, and on cooling the chains find each other again: here and there, short stretches wind back into helices that tie the chains into a network, and the water is trapped inside it. The liquid becomes a jelly. Warmed, the network comes apart and the jelly melts; cooled, it sets again. Factories extrude the jelly into strands, dry them in warm air and grind them; older works cut it into slices and dried them on nets.

## How to do it

Making gelatin from skins or bones takes long lime or acid baths, then extraction in hot water, with careful control of hygiene, which belong in a factory. Leaf gelatin from a shop shows every step after the extraction: swelling, dissolving, setting, melting and setting again.

![Three small clear glasses in a row on a wooden tray: the first holds a set, pale and clear jelly with a clean surface, the second pieces of tinned pineapple held in a firm jelly, the third pieces of fresh pineapple lying in a liquid that has stayed runny; a whole pineapple and a halved one stand behind](https://lastcodex.org/_astro/v2.CbqsU8_5_VREV0.webp)
_Fresh pineapple stops gelatin setting; tinned pineapple, already heated, does not._

Soak two or three sheets of leaf gelatin in a bowl of cold water. Within a few minutes they swell and turn soft, because the dry chains take up water without dissolving. Squeeze them, put them in a cup with a little hot water from the kettle, poured by an adult, and stir: they dissolve completely. Add cold water, with a spoonful of sugar if you like, and pour the liquid into three small glasses.

Leave the first glass as it is. Put a few pieces of tinned pineapple in the second and a few pieces of fresh pineapple in the third, then place all three in the refrigerator. The next day the first two have set and the third is still liquid. Fresh pineapple contains an enzyme, bromelain, that cuts protein chains into pieces too short to form a network; the heat used to preserve tinned pineapple has destroyed it. Finally, stand the first glass in a bowl of warm water: the jelly melts, and back in the refrigerator it sets again.

## History and evolution

In the cave of Nahal Hemar, in Israel, a human skull is covered with a thin coating that contains collagen and a resin from the storax tree, with threads of the same paste laid over it in a net pattern. The coating has been dated directly to 8920 to 8430 BCE. Baskets from the same layer, whose finds date from 8210 to 7300 BCE, carry coatings of cattle collagen on their inner and outer faces, most likely as a lining or to make them watertight. In Europe, hide glue has been identified on a yew bow from a Neolithic lakeside village in Zurich, dated to the late 4th millennium BCE. Strips of bark were stuck to it with a glue whose proteins point to the skin of cattle and of sheep or goats. In Egypt, collagen glue was used in the 3rd millennium BCE to assemble furniture and veneers and to bind paints.

Medieval cooks knew the same substance as a food. They simmered calves' feet, deer antler and meat to make broths that set into jelly, and the _Viandier_, a French cookery book of the late Middle Ages, begins its jelly with legs or feet of veal.

![Papin's digester on a small brick furnace: a squat cylindrical metal pot with a flat lid, held shut by a vertical screw in a wrought-iron yoke that grips pot and lid, and on the lid a small safety valve held down by a weighted lever; beside it on a low wooden stool a few softened bones and a bowl of jelly](https://lastcodex.org/_astro/v3.DnElAnTo_2empgC.webp)
_Papin's digester held its lid down with a screw, and a weighted valve let out excess steam, so that bones could be cooked above the boiling point of water._

In 1681 Denis Papin, working in London, described a closed pot with a lid screwed down tight, which cooked bones in water hotter than its ordinary boiling point until they softened and gave up their jelly; a French edition followed in 1682. From 1812 Jean-Pierre-Joseph d'Arcet used a process in a Paris factory that extracted gelatin from bones with the help of hydrochloric acid, which dissolves the minerals of the bone.

Gelatin then became an industrial product. In 1845 the American glue maker Peter Cooper patented a "portable gelatine", a clear jelly that could be cast in moulds. In 1871 Richard Leach Maddox proposed gelatin to hold the light-sensitive silver salts of photographic plates, and gelatin became the binder of photographic film. Today gelatin is made in large plants that steep, extract, filter, evaporate, sterilise and dry continuously, and the same steps, shorter or longer, give gelatins for food, medicine and technical uses.

## Key facts

- Collagen coating dated directly: Human skull from Nahal Hemar, Israel, 8920 to 8430 BCE
- Hide glue identified in Europe: Bow from Zurich, late 4th millennium BCE
- Papin's bone digester: Described in London in 1681
- Patent for portable gelatin: Peter Cooper, United States, 1845
- Main raw materials today: Pig skin, cattle hide, bones and fish skin

## Requires

- [Control of Fire](https://lastcodex.org/en/inventions/control-of-fire/): Light, heat and cooked food (1 million years ago)

## Sources

- [Identification of the earliest collagen- and plant-based coatings from Neolithic artefacts (Nahal Hemar cave, Israel) (Scientific Reports 6, 2016)](https://pmc.ncbi.nlm.nih.gov/articles/PMC4977467/), Springer Nature
- [Oldest Glue Discovered (21 May 1998)](https://archive.archaeology.org/online/news/glue.html), Archaeology, Archaeological Institute of America
- [Molecular evidence of use of hide glue in 4th millennium BC Europe (Journal of Archaeological Science, 2015)](https://agris.fao.org/search/en/records/65dfb69e63b8185d9cae3d6b), Elsevier
- [Manufacturing of gelatine](https://www.gelatine.org/en/gelatine/manufacturing.html), Gelatine Manufacturers of Europe
- [Gelatin as It Is: History and Modernity (International Journal of Molecular Sciences 24, 2023)](https://doi.org/10.3390/ijms24043583), MDPI
- [How glue is made (How Products Are Made, vol. 5)](https://www.madehow.com/Volume-5/Glue.html), Advameg
- [Denis Papin, biography](https://mathshistory.st-andrews.ac.uk/Biographies/Papin/), MacTutor, University of St Andrews
- [A New Digester, or Engine for Softning Bones, by Denys Papin (London, 1681)](https://ota.bodleian.ox.ac.uk/repository/xmlui/bitstream/handle/20.500.12024/A55577/A55577.html?sequence=5), Oxford Text Archive
- [More Than Just a Dessert: America's Gelatinous History, General History](https://digitalsc.lib.vt.edu/exhibits/show/gelatine/generalhistory), Virginia Tech Special Collections and University Archives
- [Improvement in the preparation of portable gelatine (US patent 4,084, Peter Cooper, 1845)](https://patents.google.com/patent/US4084A/en), Google Patents
- [Investigation: How Do Enzymes Affect Gelatin](https://www.biologycorner.com/2021/11/07/investigation-how-do-enzymes-in-pineapple-affect-gelatin/), Biology Corner
- [Jelly – will it set?](https://www.science-sparks.com/jelly-will-it-set/), Science Sparks
- [La gélatine face aux extraits et aux bouillons de viande (G. Bram and H. This, L'Actualité chimique, November 2000)](https://new.societechimiquedefrance.fr/wp-content/uploads/2019/12/2000-nov-236-NT17-Bram.pdf), Société chimique de France
- [Papin's digester: an early pressure cooker with the crucial addition of a safety valve](https://www.chemistryworld.com/opinion/papins-digester/4010391.article), Chemistry World, Royal Society of Chemistry
- [Le Viandier de Taillevent, ed. J. Pichon and G. Vicaire (1892), full text](https://www.gutenberg.org/ebooks/26567), Project Gutenberg
- [State of the (t)art: bread-like objects from the Neolithic lakeshore settlement Parkhaus Opéra, Zürich (PLOS ONE 12, 2017)](https://journals.plos.org/plosone/article?id=10.1371/journal.pone.0182401), PLOS
- [Gelatine bromide plates](https://www.cameramuseum.ch/en/discover/permanent-exhibition/the-plate-era/gelatine-bromide-plates/), Swiss Camera Museum, Vevey
- [Gelatin dry plate](https://new.graphicsatlas.org/gelatin-dry-plate), Graphics Atlas, Image Permanence Institute
- [Gelatin Handbook (pretreatment by liming or acid, then washing and extraction in hot water)](https://nitta-gelatin.com/wp-content/uploads/2018/02/GMIA_Gelatin-Handbook.pdf), Gelatin Manufacturers Institute of America

Fact-checked on 2026-10-21.

---

The Last Codex · https://lastcodex.org/en/inventions/gelatin-production/ · © The Last Codex. Texts, plates and figures: CC BY-NC-ND 4.0.