Zinc is hard to smelt because it turns to vapour at the heat needed to free it from its ore, then burns back to oxide in the air. Zinc metal was first produced by distillation in closed clay vessels. Zawar in Rajasthan was distilling zinc on an industrial scale by the early Middle Ages, China followed under the Ming, and Europe in the eighteenth century.

![Zinc Smelting · A metal that leaves the fire as a vapour and has to be caught as it cools](https://lastcodex.org/_astro/plate.CzGcKN6y_2c0Ha.webp)

## Legend

1. Firing chamber
2. Cooler lower chamber
3. Inverted clay retort
4. Perforated plate carrying the retorts
5. Condenser under the neck of a retort

## What it is

Zinc is a bluish-grey metal that is almost always found combined with other elements in its ores; native zinc, the free metal, is a very rare mineral. Its ores were long known in Europe under the single name calamine, which covered two zinc minerals, smithsonite and hemimorphite, found in the weathered upper part of ore bodies. Deeper down the usual ore is sphalerite, a zinc sulphide, often mixed with lead ores. Smelting means separating the zinc from the oxygen or sulphur it is bound to, as with copper or lead, but zinc behaves differently in the fire.

![An old galvanised steel bucket with a wire handle and a dent in its side, its silver-grey surface covered with the large flower-like crystal pattern of a hot-dipped zinc coating](https://lastcodex.org/_astro/v1.jsm1eVTJ_Z2EGN5.webp)
_A galvanised bucket: the crystal pattern on its surface is the zinc coating that keeps the steel from rusting._

Today the main use of zinc is galvanising, a thin coating that protects steel from rust. It also goes into die-cast parts, into brass, its alloy with copper, and into chemicals. Brass was made for many centuries before anyone could produce zinc metal, because the zinc of the ore could go straight into the copper without ever appearing on its own. Zinc metal was a later achievement, and it took a different kind of furnace.

The work is dangerous. The fumes of zinc oxide given off by hot zinc cause metal fume fever, with chills, fever, cough and tightness in the chest. Zinc ores often carry cadmium and lead, and roasting sulphide ores releases sulphur dioxide. Zinc smelting has always been an industrial process, with no small version that can be run safely.

## How it works

Zinc has a low boiling point. The heat needed to strip the oxygen from its ore is already above that point, so the zinc is set free as a vapour. In an open furnace this vapour rises with the hot gases, meets the air and burns back to zinc oxide, a white powder, and almost nothing is recovered. Zinc metal can therefore only be won in closed vessels, where the vapour meets no air and turns back into metal in a cooler part.

![Excavated clay retort shaped like an aubergine lying on its side, with its narrow neck, and beside it, separate, its small pot-shaped condenser; reddish fired clay blackened by fire, a grey crust inside the neck](https://lastcodex.org/_astro/v2.DpfpneNx_DD077.webp)
_A retort and its condenser of the Zawar type, as excavated._

At Zawar, in the Aravalli Hills of Rajasthan, the furnaces held rows of elongated clay retorts set upside down, their necks passing through a perforated floor into a cooler chamber below, with a clay condenser under each neck. Chinese smelters later used upright retorts with a cooler condensing zone at the top.

Distillation in closed vessels remained the way of making zinc for centuries, in India, in China and then in Europe. In the twentieth century most smelters turned to electrolysis, in which an electric current deposits zinc as metal from a solution prepared from the ore. The zinc never has to pass through the vapour stage, and this route now produces most of the world's zinc, while the gases and residues of the process still have to be captured and treated.

## History and evolution

Brass is older than zinc metal: the way of making it in sealed crucibles, without isolating the zinc, was developed in the Near East in the first millennium BCE. The earliest known large-scale production of zinc metal comes from India. Kharakwal and Gurjar argue that pure zinc was already being made in the second half of the first millennium BCE, with commercial production beginning in the early Middle Ages. Craddock and his colleagues place the start of industrial distillation at Zawar about a thousand years ago, and the Historical Metallurgy Society the twelfth century. Zawar's mines and furnaces then worked for centuries, and excavations there have uncovered the furnaces and their retorts.

China took up zinc smelting by the middle of the Ming dynasty, in the fifteenth and sixteenth centuries, using its own method of upright retorts. Excavated works along the Upper and Middle Yangtze date from that period, and a Ming treatise on crafts, the *Tiangong Kaiwu*, describes and illustrates the smelting of zinc. Chinese zinc went mostly into brass, including the brass of the copper-alloy [coins](/en/inventions/coinage/) of the empire.

![Two boat-shaped Chinese zinc ingots recovered from a shipwreck, lying on old planks, dull grey, partly covered with whitish concretions, each with a stamped mark in which no character can be read](https://lastcodex.org/_astro/v3.D_lm_GCO_Z2oKSES.webp)
_Chinese zinc ingots recovered from a wreck: Asian zinc travelled to India and Europe by sea._

From the sixteenth century, small amounts of Asian zinc reached Europe. Chinese zinc, shipped by the Dutch and English East India Companies, then dominated the world market until the nineteenth century. In 1738 William Champion of Bristol patented a way of producing zinc from calamine on a large scale, by distillation in closed retorts. He later moved to Warmley, east of Bristol, where he built a works that smelted copper and zinc and made brass and finished goods on a single site.

During the First World War the Anaconda Copper Mining Company began refining zinc by electrolysis in Montana, about 1915–1916, using the electricity of the region's hydroelectric dams to treat complex ores that were hard to smelt, and soon moved its main zinc plant to Great Falls. Electrolysis spread to most smelters during the twentieth century, and so did the use of zinc for galvanising steel, for die-cast parts and for the electrodes of many [batteries](/en/inventions/battery/).

## Key facts

- Why zinc is difficult: It turns to vapour at the heat needed to free it from its ore
- Zawar, Rajasthan: Industrial zinc distillation from the early Middle Ages
- China: Zinc smelted by the middle of the Ming dynasty, 15th–16th century
- William Champion's patent: Bristol, 1738
- Electrolytic zinc: Montana, 1915–1916

## Requires

- [Mining and Quarrying](https://lastcodex.org/en/inventions/mining/): Reaching minerals underground and keeping the workings safe (46,000 years ago)
- [Charcoal](https://lastcodex.org/en/inventions/charcoal/): Wood cooked slowly under earth (c. 4,500 BCE)
- [Pottery](https://lastcodex.org/en/inventions/pottery/): Clay turned to stone by fire (20,000 years ago)

## Sources

- [Archaeology Datasheet 204: Other metals, smelting and production of alloys](https://historicalmetallurgy.org/media/uo3lexjn/hmsdatasheet204.pdf), Historical Metallurgy Society
- [The earliest zinc artefacts, The Crucible 90 (Winter 2015)](https://historicalmetallurgy.org/media/51knpava/the-crucible-90.pdf), P. Craddock, J. Cribb, N. Gale and S. La Niece, Historical Metallurgy Society
- [Zinc and Brass in Archaeological Perspective (Ancient Asia 1, 2006)](https://ancient-asia-journal.com/articles/10.5334/aa.06112), J. S. Kharakwal and L. K. Gurjar, Ubiquity Press
- [Ancient zinc smelting in the Upper and Middle Yangtze River region (Antiquity 94, 2020)](https://www.cambridge.org/core/journals/antiquity/article/ancient-zinc-smelting-in-the-upper-and-middle-yangtze-river-region/C5960CB35D581CE96D074949B79145D3), Y. Li, B. Xiao, G. Juleff et al., Cambridge University Press
- [Not so efficient, but still distilled: the technology of Qing Dynasty zinc production at Dafengmen (Journal of Archaeological Science 43, 2014)](https://archaeology.pku.edu.cn/2014Not-so-efficient-but-still-distilled.pdf), W. Zhou, M. Martinón-Torres, J. Chen and Y. Li, Elsevier
- [China's emerging demand and development of a key base metal: Zinc in the Ming and early Qing, c. 1400–1680s (2017)](https://journals.sagepub.com/doi/10.1177/1359183517702686), H. Chen and G. B. Souza, Journal of Material Culture
- [William Champion](https://www.gracesguide.co.uk/William_Champion), Grace's Guide to British Industrial History
- [Warmley](http://www.aibt.org/warmley.html), Avon Industrial Buildings Trust
- [Purification Department of Zinc Leaching Division at Anaconda, Montana (bachelor's report, 1949)](https://digitalcommons.mtech.edu/bach_theses/306/), J. L. Brown, Montana School of Mines
- [Zinc Industry](https://www.encyclopedia.com/history/dictionaries-thesauruses-pictures-and-press-releases/zinc-industry), Encyclopedia.com (Dictionary of American History)
- [Morony Hydroelectric Facility (Great Falls Hydroelectric Facilities), written historical and descriptive data](https://tile.loc.gov/storage-services/master/pnp/habshaer/mt/mt0400/mt0476/data/mt0476data.pdf), Historic American Engineering Record, Library of Congress
- [Identification and Description of Mineral Processing Sectors and Waste Streams: Zinc](https://archive.epa.gov/epawaste/nonhaz/industrial/special/web/pdf/id4-zin.pdf), US Environmental Protection Agency
- [Zinc electrowinning from galvanized mild steel scraps](https://mineralis.cetem.gov.br/bitstream/cetem/2158/3/Zinc%20electrowinning.pdf), CETEM, Centro de Tecnologia Mineral (Brazil)
- [NIOSH Pocket Guide to Chemical Hazards: Zinc oxide](https://www.cdc.gov/niosh/npg/npgd0675.html), National Institute for Occupational Safety and Health
- [Toxicological Profile for Zinc](https://www.atsdr.cdc.gov/toxprofiles/tp60.pdf), Agency for Toxic Substances and Disease Registry
- [Zinc (Handbook of Mineralogy)](https://handbookofmineralogy.org/pdfs/zinc.pdf), Mineralogical Society of America
- [The Mineral Native Zinc](https://galleries.com/minerals/elements/zinc/zinc.htm), Amethyst Galleries, Mineral Gallery

Fact-checked on 2026-10-20.

---

The Last Codex · https://lastcodex.org/en/inventions/zinc-extraction/ · © The Last Codex. Texts, plates and figures: CC BY-NC-ND 4.0.