Fusion welding
Joining metal by melting it
Contents
- 1Welding set
- 2Electrode holder and coated electrode
- 3Earth clamp and return cable
- 4Arc and molten pool at the joint
- 5Weld bead
- 6Hand shield with a dark filter
Fusion welding joins pieces of metal by melting their edges together, usually with some added metal, so that they cool into a single piece. Bronze founders were already doing it in the 7th or 6th century BCE, pouring molten bronze between the cast parts of large statues in South Arabia and then in Greece. The heat later came from a gas flame or an electric arc: Benardos and Olszewski patented carbon-arc welding in 1885, Fouché and Picard built an oxy-acetylene torch around 1903, and coated electrodes, then gas-shielded arcs, spread welding through industry.
What it is
Fusion welding joins two pieces of metal by melting them where they meet. The edges and, most often, some filler metal run together into one pool, and when the pool freezes the two parts are a single piece of metal across the joint.
Left, a soldered joint: only the solder melts. Right, a weld: the plates themselves are fused.
Two other ways of joining metal look similar and work differently. In soldering, a filler that melts at a much lower temperature wets the surfaces and sets between them, while the parts themselves stay solid. In forge welding, the old method of the blacksmith, two pieces of iron are heated in the fire and hammered until they join, without melting. Fusion welding needs a heat source intense enough to melt the parts locally, today usually an electric arc or a gas flame.
A typical arc-welding set of the mid-20th century is built around a transformer. One cable runs from the set to the electrode holder, which grips a metal rod with a coating, the electrode. A second cable ends in an earth clamp fixed to the work. The arc burns between the tip of the electrode and the joint, over a small pool of molten metal, and leaves a weld bead behind it as the welder moves along. The welder watches through the dark filter of a shield. In the finished butt joint, the bead fills the gap and the fused zone reaches into both plates.
How it works
When the electrode is brought close to the work, current jumps the small gap through a column of hot, ionised gas, the arc. The arc is hot enough to melt the tip of the electrode and the edges of the joint. Drops of metal from the electrode cross the arc into the pool, so the electrode is used up as the weld grows. Its coating melts as well and gives off gas and a layer of slag that cover the molten metal and keep air away from it; the slag is chipped off the bead once it has cooled. The circuit runs from the set through the holder, the arc, the work and the earth clamp back to the set.
A gas-welding outfit: oxygen and acetylene are mixed in the torch.
Gas welding uses a flame instead. Oxygen and acetylene come from two cylinders through regulators and hoses and mix in the torch. In 1895 Henri Le Chatelier obtained a flame of about 3000 °C by burning the two gases together. The welder melts the edges of the joint with the flame and feeds a filler rod into the pool by hand. Unlike the arc, gas welding needs no electricity.
Later arc processes protect the pool with a gas instead of a coating. In TIG welding, perfected in 1941, an electrode of tungsten that does not melt makes the arc under a stream of inert gas, and the filler is added separately. In MIG welding, developed in 1948, a wire fed continuously through a gun is both electrode and filler.
Every form of welding is dangerous work. The arc gives off ultraviolet light that burns the eyes and skin, which is why the shield carries a dark filter and welders wear gloves and covering clothes. The fume of melted metal and coating causes cancer: the International Agency for Research on Cancer classed welding fume as carcinogenic to humans in 2017, and the British Health and Safety Executive now expects it to be extracted at the source. Arc sets carry the risk of electric shock, gas cylinders and hoses can feed fires, and sparks and hot metal set alight anything nearby. Welding equipment is used by trained welders, with fume extraction, screens and fire precautions.
History and evolution
Benoît Mille has identified flow fusion welds on Hawtar’athat, a large bronze statue from South Arabia that its inscription dates to the late 7th or first half of the 6th century BCE. In Greece, the oldest fusion welds identified so far are on large bronzes. Statues of life size or more were cast in several pieces by the lost-wax process and then joined, and Aurélia Azéma and her colleagues date the earliest Greek welds to the late 6th or early 5th century BCE, the time of the first large bronze statues. The founders poured molten bronze into a channel cut along the joint or into a gap left between the two parts, so that it melted their edges and fused with them.
Oval basins along the join of an arm, where molten bronze was poured in.
On some statues, such as the Riace bronzes, the welds show as a line of oval basins along the joint. Angelini, Artioli and their colleagues have analysed the lead isotopes of samples taken from the welds of the Riace bronzes. In laboratory trials, Azéma’s team could not make a weld longer than a few centimetres, while some ancient welds are up to a metre long, and they suspect that the founders used an additive that acted as a flux. Smiths had joined metal long before without melting it. Miller and TWI both mention small gold boxes of the Bronze Age with welded joints, which Miller says were made by pressing lapped edges together. Hot iron was joined by forge welding, hammering two pieces until they bond: Nurcan Küçükarslan reports traces of it in Middle Bronze Age iron objects from Kaman-Kalehöyük in Anatolia, and TWI notes that it remained the usual way of welding iron until the 19th century.
The electric arc made new kinds of welding possible. Humphry Davy showed an arc between carbon electrodes early in the 19th century; TWI dates it to 1800, Miller to 1809. In 1881 Auguste de Méritens used the heat of an arc to join the lead plates of storage batteries. Nikolai Benardos and Stanislaus Olszewski patented welding with a carbon electrode in Britain in 1885 and in the United States in 1887. Nikolai Slavyanov in Russia in 1888 and C. L. Coffin in the United States in 1890 used a metal electrode that melted into the joint.
Gas welding grew alongside. After Le Chatelier’s work on the oxy-acetylene flame, the French engineers Edmond Fouché and Charles Picard developed a torch to burn the two gases, dated 1903 by Metinvest. Miller places a torch suitable for low-pressure acetylene around 1900. Between 1907 and 1914 the Swede Oscar Kjellberg invented the coated electrode. The demand for armaments in the First World War spread welding through industry, and by the late 1930s shipyards were using automatic arc welding under a layer of flux.