Eyeglasses
Lenses that extend a working life
Contents
- 1Biconvex glass lens
- 2Bone rim
- 3Handle
- 4Iron rivet
- 5Copper wire binding
Loading the figure…
Eyeglasses are a pair of lenses held in a frame in front of the eyes to correct presbyopia, long sight, short sight or astigmatism. They appeared in Italy in the 1280s as reading aids for older people; lenses for short sight followed in the fifteenth century and side arms in the eighteenth.
What it is
Eyeglasses, or spectacles, put a lens in front of each eye so that the light reaches the retina already bent by the right amount. The first ones helped people in their forties and older to read and to do fine work, once focusing at reading distance had become hard.
The pair on the plate is the oldest type, the rivet spectacles of the fourteenth and fifteenth centuries. Each glass lens sits in a ring carved from bone, wood or horn. A short handle sticks out from each ring, and the two handles are joined by a single rivet. The pair has no side arms: the rivet rests on the bridge of the nose and the rims pinch the nose on either side, so the wearer has to keep the head level or hold the spectacles with one hand.
How it works
A reading stone, a dome of crystal or glass laid on the page, was the magnifier that came before spectacles.
Inside the eye, a soft lens changes shape to bring near or distant things into focus. With age it hardens, and the closest point the eye can see sharply moves away: a few centimetres from a child’s face, it ends up out of reach of the arms for most people of sixty. This is presbyopia, and it is why reading glasses were the first ones made.
A convex lens, thicker in the middle than at the edge, makes the light converge a little before it enters the eye, and so does part of the work that the eye’s own lens can no longer do. Opticians measure this power in dioptres, the inverse of the focal length in metres. A reading lens of +2 dioptres brings parallel light to a point 50 cm behind it.
Short sight is a different focusing problem, and it can come on top of presbyopia. The eyeball is a little too long, or its optics too strong, and distant things blur. A concave lens, thinner in the middle, spreads the light slightly before it enters the eye and pushes the image back onto the retina. Lenses of this kind were being ground in Florence in the fifteenth century. In astigmatism the eye’s power differs between two perpendicular directions, so lines at one angle blur more than lines at another. Correcting it needs a lens curved more in one direction than the other, and such lenses came much later.
How to do it
A pair of rivet spectacles like the one on the plate takes two lenses, a piece of bone or hardwood, copper wire and one small rivet.
The glass blank, fixed with pitch to a wooden handle, was worked with wet abrasive in a bronze tool, then polished on leather.
Get the lenses. For a pair you will actually look through, take two lenses from a cheap pair of modern reading glasses. Grinding your own is a historical demonstration: as a spectacle maker did, rub a disc of glass about 4 cm across with wet abrasive powder inside a tool hollowed to the curve you want, finishing with finer and finer grits, then polish it with rouge on leather or felt. For a +2 dioptre lens made of ordinary glass, both faces need a radius of curvature of about 50 cm, a very shallow curve. Hand-ground lenses will not have an exact power, and their optical centres will not be lined up with your pupils.
Cut the rims. Mark two circles on a flat piece of bone or boxwood with dividers, a little larger than the lenses, and saw them out with a fine saw, leaving a short tab on each ring for the handle. Cut a V-shaped groove around the inside of each rim to hold the edge of the lens.
Split and bind. Saw through each rim on the side opposite the handle. Spring the ring open, slide the lens into the groove and close the split by wrapping thin copper wire several times around two small lobes left on either side of it.
Rivet the handles. Drill a small hole near the end of each handle, overlap them and set a copper or iron rivet, peened just tight enough that the two halves can still be folded. File small notches along the inner edges where the rims meet the nose, so they grip better.
Safety. Never look at the Sun through a lens, and never leave one in sunlight near paper or wood, because it can start a fire. This pair is a replica: do not use it in place of glasses prescribed and fitted by an optometrist, and never drive with it.
History and evolution
Polished crystals and glass had been used to enlarge writing long before spectacles. The step of setting a lens in a frame in front of each eye came in Italy around 1280 to 1290. Where exactly is not known: Pisa and Florence are often proposed, and a Venetian ordinance of 1300 already punished glassmakers who sold glass “discs for the eyes” as rock crystal. In a sermon given in Florence in 1306, the Dominican friar Giordano da Pisa said that the art of making spectacles was not yet twenty years old and that he had spoken with the man who first made them. Nobody knows his name.
The oldest known painting of spectacles is a fresco of 1352 by Tommaso da Modena in the chapter house of San Nicolò in Treviso, which shows a Dominican cardinal reading with rivet spectacles. Real frames rarely survive. A bone pair from the fifteenth century was found at Trig Lane, by the Thames in London, at a time when thousands of spectacles a year were imported into London from the Low Countries. In the 1460s the dukes of Milan ordered spectacles from Florence by the dozen, the reading lenses graded by age from thirty to seventy, a sign that lens strengths had become fairly standard.
Double spectacles of the late eighteenth century: a distance lens above, a reading lens below.
By the early sixteenth century spectacles could correct short sight as well as long sight, and bridges of leather or whalebone replaced the rivet. Around 1730 the London optician Edward Scarlett is credited with adding rigid side arms, or temples, that pressed against the sides of the head. In letters of 1784 and 1785 Benjamin Franklin described his “double spectacles”, with half of each lens for distance and half for reading. Pince-nez, held by a spring on the nose, followed in the nineteenth century, then in the twentieth plastic frames, lighter plastic lenses and, later, thinner high-index lenses.